IMPORTANT: Texsource ships in-stock items as orders are placed, and cannot guarantee that temperature-sensitive items, like emulsions and emulsion removers, will not be exposed to freezing temperatures in transit. Texsource is not responsible for items damaged by exposure to extreme temperatures.
SAATI SAATItex PHU-MT emulsion is a pure photopolymer emulsion that is universally suitable for most inks, including solvent, water-base and plastisol.
Features and Benefits
Dyed blue
One-part pure photopolymer emulsion with universal ink resistance.
Exposes approximately 8x faster than typical two-part emulsion
45% solids
High viscosity easily coats all mesh counts
Easy to reclaim
Can be used with solvent based, UV and water based inks, without using diazo.
Can be used with Diazo 11 when extra sharpness or high resolution is required*
DIRECTIONS FOR USE Handle under yellow safelight or low wattage tungsten lights. Avoid exposure to daylight, quartz/halogen lamps, cool white fluorescent lamps or discharge lamps.
Sensitizing & Mixing Emulsion is presensitized during production and does not require mixing.
Mesh Preparation & Degreasing
Degrease and abrade new mesh with Saatichem Direct Prep 1 in order to optimize stencil adhesion; dry and store the screen in a dust free, dry environment prior to coating. For more applications, thoroughly degrease mesh prior to use with Saatichem Direct Prep 2.
Coating Using a high quality scoop coater or coating through, apply one or two coats to the substrate side of the screen, followed by one or two coats on the squeegee side. For a thicker stencil, apply additional coats to the squeegee side prior to drying. For a higher quality stencil with a minimal increase in stencil thickness, apply one or two additional coats to the substrate side of the screen after the initial coats have dried.
Drying & Storage Thoroughly dry the coated screen at a maximum temperature of 104°F (40°C) in a dust free, dark or yellow light area, with the substrate side facing down to optimize stencil quality. Coated screens should be stored in a dust free, dry, safelight environment.
Exposing Ensure that all surfaces, emulsion, film and glass are free of dust to minimize pinholes. Contact the emulsion side of the positive with the substrate side of the screen and secure in position before placing the screen in a suitable vacuum frame. Many variables, such as lamp type and age, distance from lamp to screen, mesh type and coating thickness, can affect exposure time. Perform an exposure test with an exposure calculator to determinate correct exposure time for a complete cure.
Developing Wet both sides of the screen with a strong, finely divided spray of water and continue washing out until all image areas are fully open. Rinse both sides of the screen and dry thoroughly before use. A properly exposed and developed screen will not leave residues on the squeegee side.
Post Exposing Post expose with daylight or exposure lamp to produce a more water-resistance stencil.
Reclaiming Remove all ink residues immediately after printing with an appropriate solvent. Remove stencil with Saatichem Remove ER1, ER2, ER4, ER5 or ER10 and a pressure washer. For stains and ghost images, use Saatichem Remove HR3 followed by a pressure washer.
Health & Safety Before using, refer to appropriate material safety data sheets.
Shelf Life - When sealed in the original container and stored in cool conditions, SAATI products will maintain their original properties for one year from the date of production.
Emulsion Exposure Differences
Proper screen exposure must take many factors into account – the emulsion type, coating thickness, exposure unit, etc. As a general guideline for the different emulsion types (diazo, dual cure, and photopolymer) use these times as a reference.
Photopolymer – These are typically the fastest exposing emulsions, with many exposing correctly from 30-50 seconds. The shortest times can be seen when using a newer LED-type exposure unit.
Dual Cure – If you have established a good exposure time with photopolymer emulsions, you can typically add 90 seconds (1.5 minutes) to that time for most dual cure emulsions.
Diazo - If you have established a good exposure time with photopolymer emulsions, you can typically add 210 seconds (3.5 minutes) to that time for most diazo emulsions.
These times will depend heavily on your exposure unit and should only be considered as a starting point.
NOTE - The product image is intended to show an approximate color of the product when applied to the screen. Actual color may vary. Product listing does not include screen and / or scoop coater.
See something that brings up a question? Contact us toll-free at 888-344-4657 (habla español), catch us on any of our social media accounts, or send us an email. We are here to serve you, and we look forward to hearing from you!
*Free Shipping - Our Free Shipping offer applies to any online order over $299 that contains eligible items (denoted by the Free Shipping banner under the product price). Generally this will apply to regular Stock supply items but may also include equipment if noted on that product page. Non-stock items may be shipped directly from the manufacturer and are not eligible for free shipping. Orders combining free and non-free shipping items will only be charged by the weight of the non free-shipping items. Free Shipping offer is only valid for orders delivered to continental US addresses. All free shipping orders will be shipped standard ground via best rate carrier. Our Free Shipping promotion does not cover additional UPS or FedEx fees such as Overweight Packages.
Texsource makes every effort to keep our website information accurate and up to date. However, Texsource is not responsible for errors in pricing and/or product descriptions, or alterations from displayed photos. If you have a question concerning such a product, please feel free to contact us.
All images, sounds, video, and graphics contained within this site are used as either property of Texsource, used under license, or used with permission. If you feel that an asset does not meet this requirement please email webmaster for inquiry or takedown request.
NOTE - Additional freight charges may be applied to your order for equipment purchases, special order items, motor freight shipments, crating fees, or dropship items that may incur shipping and handling fees that may not be known at the time of the order.